Enhance Oil Recovery Used PHPA

Enhance Oil Recovery Used PHPA

PHPA is applicable in freshwater, seawater, saturated saltwater mud, KCl and solids free brine systems.It provides cuttings encapsulation, shale filming/inhibition, flocculation of drilled solids, viscosity and lubricity.
Description
Technical Parameters

 

Enhanced Oil Recovery(EOR) used PHPA

Welcome to consult enhance oil recovery used phpa price with Shandong Tongli Chemical Co.,Ltd, which is one of the leading enhance oil recovery used phpa suppliers in China and also a productive phpa enhance oil recovery, eor enhance oil recovery, enhance oil recovery eor factory.

76.jpg

EOR Used PHPA

I. Description

Enhanced Oil Recovery PHPA is a specially treated high molecular weight Partially Hydrolyzed Polyacrylamide polymer for all water-base drilling fluids. It functions as viscosifying agent, shale and bore-hole stabilizer, encapsulator, bentonite extender, flocculation agent and assist with fluid loss control.

II. Application & Features

Enhanced Oil Recovery PHPA is applicable in freshwater, seawater, saturated saltwater mud, KCl and solids free brine systems.It provides cuttings encapsulation, shale filming/inhibition, flocculation of drilled solids, viscosity and lubricity.

PHPA's strong encapsulating/filming action stabilizes clay and shale formations, blocks the absorption or inhibition of water from the drilling fluids, prevents clay and shale cuttings from disintegration and dispersion into the mud while carrying up the annulus from bit to surface.

Fluids contained PHPA has property of shear-thinning which helps maximize drill rate by exhibiting low bit viscosity and high lifting capacity at the lower shear rate at the annulus.


Items

Anionic Polyacrylamide

Specifications

Results

Characteristics

Appearance

White Powder

White Powder


Filtration ratio

≤2.0

1.3


Toxicity

Non-toxic

Non-toxic

Apparent viscosity , mPa.s

≥12.5

16.0

Shear viscosity retention rate,%

≥80.0

87.0

Static adsorption viscosity retention rate,%

≥80

85.0

Residual acrylamide content,%

≤0.1

0.05

Interfacial Elastic Modulus,Mn/m

E’≥38

39

Intrinsic viscosity,ml/g

≥2200

2210

Disslove Time, minute

≤90

60


IV. Packaging

Enhanced Oil Recovery PHPA 25Kg triple composite /PE Bag, it can also be customized packaging.